  • Fig. 3 Mechanical tests on varying wall thickness and relative density samples.

    (A to D) Stress-strain plots of structures with varying wall thicknesses in showing the transition from brittle to ductile-like deformation in thinner-walled structures. (E to J) Post-compression images of the nanolattices showing the recoverability as wall thickness is reduced.